Sign In | Join Free | My burrillandco.com
Home > Precision alloy product >

N-155 Superalloy, Multimet R30155 Cobalt Alloy Rod

    Buy cheap N-155 Superalloy, Multimet R30155 Cobalt Alloy Rod from wholesalers
     
    Buy cheap N-155 Superalloy, Multimet R30155 Cobalt Alloy Rod from wholesalers
    • Buy cheap N-155 Superalloy, Multimet R30155 Cobalt Alloy Rod from wholesalers

    N-155 Superalloy, Multimet R30155 Cobalt Alloy Rod

    Ask Lasest Price
    Brand Name : AIWEN
    Certification : SH
    Model Number : SH-N-155
    Price : Available per request
    Delivery Time : 25-30DAYS
    Payment Terms : T/T
    Supply Ability : 100000 KG per year
    • Product Details
    • Company Profile

    N-155 Superalloy, Multimet R30155 Cobalt Alloy Rod

    N-155 Superalloy, Multimet R30155 Cobalt Alloy Rod

    Features of N-155 Superalloy, Multimet R30155 Cobalt Alloy Rod:

    *N-155 alloy has high temperature properties which are inherent and do not depend upon age hardening
    *It is recommended for applications involving high stresses at temperatures up to 1500°F, and can be used up to 2000°F where only moderate stresses are involved
    *It has good ductility, excellent oxidation resistance, and can be readily fabricated and machined

    Applications of N-155 Superalloy, Multimet R30155 Cobalt Alloy Rod:

    It is commonly used for high-temperature bolts and aircraft parts, including:
    *Tail pipes and cones
    *Exhaust manifolds
    *Nozzles
    *Turbine, combustion chamber and afterburner components

    Quality N-155 Superalloy, Multimet R30155 Cobalt Alloy Rod for sale
    Inquiry Cart 0
    Send your message to this supplier
     
    *From:
    *To: Suzhou Xunshi New Material Co., Ltd
    *Subject:
    *Message:
    Characters Remaining: (0/3000)